Skip to content
by IQAC KIITKIIT Deemed to be University — Internal Quality Assurance Cell

Publication2025

Electrical discharge machining of Ni-based superalloy and its applications in aero turbine parts: a comprehensive review

The record

Type
Publication
Date
1 January 2025
Level
National
Journal
Advances in Materials and Processing Technologies
Volume
11
Issue
2
Pages
1085-1121
Published
1 January 2025
DOI
10.1080/2374068x.2024.2358638
Scopus ID
85195208911
ISSN
2374068X
Authors
3
Open access
No
Citations
17
International co-authorship
No
Co-author countries
IN

Classification

Every label below carries the reasoning it was assigned on, the confidence band it was assigned in, and what produced it. The rubric is published.

UN Sustainable Development Goals

  1. 9.4 Upgrade infrastructure and retrofit industries to make them sustainable and resource-efficient

    TargetPrimaryModerate confidenceJudged

    Review of electrical discharge machining techniques for nickel-based superalloy aero-engine components addresses surface integrity and precision manufacturing.

    Moderate confidence
    The alignment is plausible and defensible but rests on an assumption a reasonable reviewer could decline. Published, and surfaced in the review queue for a human to confirm or override.
    Judged
    Judged against the published classification rubric, under the rubric and prompt versions recorded with the run that produced it.
    Produced by
    claude-haiku-4-5-20251001, under kortex-publication-v1

Viksit Bharat @2047

  1. vb-3 Innovation, Science and Technology

    ThemePrimaryModerate confidenceJudged

    Derived through the seeded SDG-to-Viksit-Bharat crosswalk from the primary SDG 9 label. Review of electrical discharge machining techniques for nickel-based superalloy aero-engine components addresses surface integrity and precision manufacturing.

    Produced by
    claude-haiku-4-5-20251001, under kortex-publication-v1

Each label above carries the instrument and the version that produced it. How each classification is reached.

Evidence

Kortex hosts no documents. Evidence is an outbound link to the authority that holds it.

No outbound evidence link is recorded for this activity. The record below states which source it came from and when it was last read.

Provenance

Which source system this record came from, how many source rows were resolved into it, and when each was last read.

Source rows resolved into this record
1

Each record carries the date Kortex last read it from its source system. That is a freshness date and not a verification: Kortex records what its sources say and when it read them, and it does not check those statements against any external authority. No claim on this site is described as verified, because none is.

Citing this record

This URL is stable. A record’s permalink is frozen when it is published and is not regenerated if its title is later corrected.

KIIT Deemed to be University. “Electrical discharge machining of Ni-based superalloy and its applications in aero turbine parts: a comprehensive review”. Kortex.

Explore the full record